How to Speed Up Screed Drying Safely

When the programme is tight, everyone wants the screed dry sooner. There are sensible ways to help drying along, and there are shortcuts that cause cracking, curling and failed floors. This guide from the Screed Scientist explains the difference.

Start with the basics

Before reaching for equipment, get the building conditions right. Screed dries by moisture moving up through it and evaporating from the surface into the air. Anything that helps the air carry that moisture away will help drying.

  • Make the building weathertight. Keep rain and wind-driven moisture out.
  • Keep conditions steady. Avoid big swings in temperature and humidity.
  • Ventilate, once the screed allows it. Moving air carries moisture away from the surface. Follow the manufacturer’s guidance on when to open the building up, as some screeds need protecting from fast drying early on.
  • Keep other wet trades in mind. Plastering and other wet work in the same space raise humidity and slow drying.

Force drying flowing screed

One advantage of flowing screed is that it can be force dried after 7 days. Force drying is not suitable for traditional sand and cement screed, which must be left to dry naturally. Common methods include:

  • Dehumidifiers. These take moisture out of the air, so the air can take more moisture from the screed. Close the room up while they run so they aren’t trying to dry the outside air.
  • Underfloor heating. Where it is installed, heating can help drying, but it must be brought up gradually and in line with the screed and heating manufacturers’ commissioning guidance.
  • Gentle air movement. Fans can help move damp air away from the surface.

Always check the screed manufacturer’s guidance first. Proprietary products can have their own instructions and timings.

The mistakes to avoid

Drying too fast or too unevenly can damage a screed. Common mistakes include:

  • Turning the heating up full straight away. Sudden heat dries the top quickly while the body of the screed stays wet. That can lead to cracking or curling, and the readings can be misleading.
  • Using underfloor heating before commissioning guidance allows. Follow the heating and screed manufacturers’ procedures.
  • Blasting direct heat onto one area. Gas heaters and space heaters can add moisture to the air, and focused heat dries patches unevenly.
  • Testing straight after force drying. If the surface has just been dried hard, it can give a false impression. Allow conditions to settle and test as the manufacturer advises.
  • Assuming faster drying means it’s ready. However you dry the screed, the only way to know it’s ready is to test it.

Reinforcement can help to control cracking in some screeds, but it isn’t a substitute for sensible drying.

Surface DPMs: a different option

Sometimes the programme simply can’t wait for a screed to dry naturally. In that case, a surface DPM (damp-proof membrane) may be an option. A surface DPM is a coating laid on top of the screed that suppresses moisture and controls moisture evaporation so that it isn’t harmful to sensitive floor finishes.

A surface DPM doesn’t dry the screed. It manages the moisture so the finish is protected. The choice of product, preparation and application should follow the manufacturer’s instructions, and the flooring contractor and floor covering manufacturer should agree that it’s suitable for the finish being laid.

Test before you lay

Whichever approach you take, measure before any floor finish goes down. Use the hygrometer test or the calcium carbide (CM) test, check results against the manufacturers’ acceptable readings, and keep records. See How to Test Screed Moisture Properly. BS 8204 and BS 8203 give further guidance.

In short

  • Get the building weathertight, keep conditions steady and manage ventilation.
  • Flowing screed can be force dried after 7 days, following manufacturer guidance.
  • Bring heat up gradually and avoid drying the surface too fast.
  • A surface DPM can suppress moisture where waiting isn’t possible.
  • Always test before laying.

Next in the series: Avoiding Disputes: Records and Sign-off

Want More Expert Insights?

Explore our comprehensive library of screeding knowledge and technical guidance.